ASTM D6677-07 X-Cut Pull-Off Test - TEC Services, Atlanta, GA
In this test, an X cut is made in the coating. Tape is placed over the intersection of the cut and quickly removed with extreme force.
Storm Greeter scored perfect 10s!
What does it take to score a 10?
ASTM Standard - Coating is extremely difficult to remove; fragments no larger than approximately 0.8 by 0.8 mm (1/32 by 1/32 in) removed with great difficulty.
|